Why do injection parts have dents and shrinkage marks?

2024-10-15 09:01:28 Injection parts
The main reasons for the occurrence of depressions and sink marks in injection-molded parts are as follows:

I. Material Factors


  1. Large Material Shrinkage Rate
    Different plastic materials have different shrinkage rates. If a material with a relatively large shrinkage rate is selected, during the cooling process after injection molding, it is likely to undergo a large volume shrinkage, thus leading to the appearance of depressions and sink marks.
    For example, some crystalline plastics such as polyethylene (PE) and polypropylene (PP) have relatively large shrinkage rates. In contrast, amorphous plastics such as polystyrene (PS) and polycarbonate (PC) have smaller shrinkage rates. When selecting materials, according to the specific requirements and usage environment of the product, a material with a smaller shrinkage rate should be reasonably chosen to reduce the generation of depressions and sink marks.

  2. Poor Fluidity
    If the fluidity of the plastic material is poor, it will result in insufficient filling of the mold cavity during the injection molding process, especially in parts with a large wall thickness or complex structures, where a lack of material is likely to occur. During the cooling process, due to the lack of sufficient material replenishment in these parts, depressions and sink marks will be formed.
    The fluidity of the material can be improved by adjusting the material formula, adding lubricants, or increasing the processing temperature. For example, adding an appropriate amount of flow aids to the material can reduce the viscosity of the material, improve its fluidity, and make it easier for the material to fill the mold cavity.


    injection mould

II. Mold Factors


  1. Unreasonable Gate Size
    If the gate size is too small, it will limit the flow rate and flow volume of the plastic melt, resulting in insufficient filling of the mold cavity. Especially in the parts far from the gate, depressions and sink marks are likely to occur.
    If the gate size is too large, excessive heat will be generated at the gate of the plastic melt, causing the material to cool and solidify prematurely, affecting the subsequent filling and pressure holding processes, and also making it prone to depressions and sink marks.
    The size and position of the gate should be reasonably designed according to factors such as the size, shape, and wall thickness of the injection-molded part. Generally, the gate size should be moderate, which can not only ensure the smooth flow of the plastic melt but also avoid excessive heat generation and pressure loss.

  2. Uneven Mold Temperature
    Uneven mold temperature will cause uneven shrinkage of the injection-molded part during the cooling process, resulting in depressions and sink marks. For example, if the local temperature of the mold is too high, the plastic melt in this part will cool slowly and shrink more; while if the local temperature of the mold is too low, the plastic melt in this part will cool too quickly and shrink less.
    The uniformity of the mold temperature can be improved by optimizing the cooling system of the mold. For example, setting up a reasonable cooling water channel in the mold to ensure that the flow rate and volume of the cooling water are uniform, so as to keep the temperature of each part of the mold consistent. At the same time, equipment such as heating rods or oil temperature machines can also be used to heat the mold to improve the temperature uniformity of the mold.

  3. Unreasonable Cavity Design
    Uneven wall thickness of the cavity will lead to uneven shrinkage of the injection-molded part during the cooling process, resulting in depressions and sink marks. For example, the part with a larger wall thickness shrinks more, and the part with a smaller wall thickness shrinks less, and depressions and sink marks are likely to occur at the position where the wall thickness changes.
    When designing the cavity, the wall thickness should be kept as uniform as possible to avoid large changes in wall thickness. At the same time, the surface finish of the cavity should be improved, and the surface roughness should be reduced to reduce friction and improve the fluidity and filling ability of the material.

III. Process Factors


  1. Insufficient Injection Pressure
    Insufficient injection pressure will lead to insufficient filling of the plastic melt in the mold cavity, especially in parts with a large wall thickness or complex structures, where depressions and sink marks are likely to occur.
    The injection pressure can be appropriately increased to increase the flow rate and filling ability of the plastic melt and ensure sufficient filling of the mold cavity. However, it should be noted that too high injection pressure will also lead to other problems, such as flash and difficult demoulding. Therefore, the injection pressure should be reasonably adjusted according to the specific situation.

  2. Insufficient Cooling Time
    Insufficient cooling time will cause the injection-molded part to have a too high temperature when demoulding, and it has not been completely solidified. Thus, it will continue to shrink during the cooling process, resulting in depressions and sink marks.
    The cooling time can be appropriately extended to ensure that the injection-molded part is completely solidified before demoulding and reduce shrinkage. However, too long cooling time will also reduce production efficiency. Therefore, the cooling time should be shortened as much as possible on the premise of ensuring product quality.


In conclusion, the generation of depressions and sink marks in injection-molded parts is the result of the combined action of multiple factors such as materials, molds, and processes. In actual production, according to the specific situation, these factors should be comprehensively analyzed, and corresponding measures should be taken to reduce the generation of depressions and sink marks and improve the quality of injection-molded parts.

injection mould


Home
Product
News
Contact
主站蜘蛛池模板: 老子影院午夜伦不卡| 免费无码一区二区三区蜜桃| 久久国产高潮流白浆免费观看| 少妇极品熟妇人妻| 18国产精品白浆在线观看免费| 国产精品永久免费视频| 成a人片亚洲日本久久| 亚洲第一极品精品无码久久| 国产精品夜间视频香蕉| 又粗又猛又黄又爽无遮挡 | 亚洲欧美一区二区三区日产| 亚洲午夜久久久影院| 国产在线aaa片一区二区99| 少妇精品导航| 精品国产va久久久久久久冰| 亚洲精品成人网站在线观看| 中国人妻与老外黑人| 国产精品久久无码一区| 国模叶桐尿喷337p人体| 亚洲精品成人a在线观看| 成年在线网站免费观看无广告| 日韩精品少妇无码受不了| 国内高清久久久久久| 国模冰莲极品自慰人体| 成人a毛片免费观看网站| 久久人人爽人人爽人人片av东京热| 久久久亚洲精华液精华液精华液| 野花香视频在线观看免费高清版| 精品人妻av区乱码| 国产午夜毛片v一区二区三区| 国产精品国产自线拍免费软件| 人妻少妇精品视频三区二区一区| 精品国产乱码久久久久久浪潮| 玩弄丰满少妇人妻视频 | 日韩高清在线中文字带字幕 | 欧美内射深喉中文字幕| 国产又色又爽又黄的在线观看| 国产精品无码a∨精品影院| 国产成熟女人性满足视频| 丰满少妇呻吟高潮经历| 精品久久久久久综合日本|